Date:2025-08-12 Views:1002
C % | Ni% | Cr% | Nb% | Mn% | Si% | Cu% | Fe % |
≦0.07 | 3 - 5 | 16 - 18 | 0.15 - 0.45 | ≦1.0 | ≦1.0 | 3. 5- 4.5 | Bal. |
Parameter | Unit | Typical Value | Reference Range | Testing Method |
Melt Index | g/10min | 100 | 80 - 200 | ISO 1133 (190 ℃, 21.6Kg) |
Green Density | g/cm³ | 5.40 | 5.35 - 5.45 | ISO 3369 |
Sintered Density | g/cm³ | 7.70 | 7.65 - 7.75 | ISO 3369 |
Mold Factor | 1.165 | 1.163 - 1.168 | Mold Dimension / Product Dimension |
Sintered State | Thermally Treated State | |
Density | ≥7.70g/cm³ | |
Yield Strength | ≥730MPa | ≥960 MPa |
Tensile Strength | ≥960MPa | ≥1150 MPa |
Elongation | ≥5% | ≥4.5% |
Hardness | 220-320 HV10 | ≥380 - 400 HV10 |
Multi purpose stainless steel material. Applied to medical devices, automotive parts, tools, machinery, etc. This material is suitable for the molding and processing of relatively large MIM parts.